AISI 410

Typically supplied in the hardened and double tempered condition (197-237HBW/*22 HRC max)

Grade is typically used for pressure containing applications such as valve bodies, tubing hangers, it is also used for valve gates and stems.
Good weldability, and so may be welded to itself or weld inlayed. The grade does require a post weld heat treatment at 621oC min in order to meet sour service (NACE MR017/ ISO 15156) requirements.
Non-NACE condition hardened and single tempered product can be supplied where applications call for 105K min yield, however this condition significantly reduces the impact toughness.


Equivalent/Similar Standards

StandardMaterial Name
AISI410
WNR1.4006
CommercialEN56A
EN58
British AerospaceBS 3S61
BS S141
Military AMS 5613
MIL-L-24128
MIL-L-862B 403
MIL-S-862B 410
UNSS41000
EU ENX12Cr13
USA410
France AFNORZ10C13
UK BS410S21
Sweden SS2302
Poland PN1H13
Russia GOST12KH13
15KH13L